Nanomaterial Information

Symbol RGO
Name Reduced graphene oxide
Source Prof. Ajayan’s lab, Rice University


Dispersant  -
Size N/A
Aggregate Size[1] 684.4 ± 90.4 nm
ENM
electrophoretic
mobility[2]
-2.53 µm/(V/cm)-s 
Refractive Index 2.2

Toxicity test method

Suspension preparation method
10 mg / 50 mg RGO was added to 10 mL/50 mL ultrapure water generated by a Barnstead EPure system (Thermo Fisher Scientific, Waltham, MA) in a 10 -mL / 50 -mL centrifuge tube, and sonicated in a sonicating cup horn (sonics & Material, Newtown, CT) at 100 W for 30 min. The samples were stored at room temperature in 10 -mL / 50 -mL centrifuge tubes wrapped in aluminum foil before use within 6 months.

Particle size measurement method

ENM electrophoretic mobility measurement.

 

Footnotes:
  1. Number mean hydrodynamic diameter nm. Measured by dynamic light scattering (Zetasizer Nano, Malvern, Worcestershire, UK)
  2. Measured at ~pH 5.